· 離子濺射納米混合涂層:
·
·
· Properties of coating: typical thickness 2.0-3.0μm; friction coefficient between £ 0.15 (typically 0.05 and 0.10) against WC/Co ball; hardness H Plast. 31200kg/mm2, dark grey in colour; wear rate(SWR): 2.0E-16m3/Nm(WC-6%Co ball ?5mm, 80N test, ?8mm track, 477rpm, 30mins)
鍍層的性質:一般厚度大約2.0-3.0 μm;摩擦系數小于 0.15。(典型為:0.05-0.10間)(against WC/Co ball);硬度Hp > 1,200kg/mm2 ;深灰黑色;劃痕粘接力:大于60N;相對磨損率:2E-16 m3/Nm (WC-6%Co ball ?5mm, 80 N test ?8mm track, 477rpm, 200mms-1)。
· MoS2基鍍層一般厚度大于1.0 μm;摩擦系數約為0.05 到 0.10之間(against WC/Co ball);在150kgf的洛氏硬度計壓頭壓入,鍍層不脫落(>HF2),硬度約 950-1050 VHN;深灰色;劃痕粘接力:大于60N;相對磨損率:2E-16 m3/Nm (WC-6%Co ball ?5mm, 40 N test ?8mm track, 477rpm, 200mms-1)。
?MoST : Properties of coating: typical thickness>1.0μm; friction coefficient between 0.05 -0.10 against WC/Co ball; hardness H Plast. >950 kg/mm2, dark grey in colour; wear rate(SWR): 2.0E-16m3/Nm(WC-6%Co ball ?5mm, 80N test, ?8mm track, 477rpm, 30mins)
· CrN coating
CrN 鍍層
CrN: 鍍層硬度Hf>2000HV,鍍層厚度>3微米;結合力:在150kgf的洛氏硬度計壓頭壓入,鍍層不脫落(>HF2); 標準劃痕試驗:Lc>60N;鍍層前后的表面粗糙度增加值Ra≤0.01微米,鏡面效果。
CrN coating, the hardness of the coating: Hf>2000Hv, the thickness of the coatings: >3.0um. The adhesion of the coatings: >HF2. And Lc > 60N with Scratch system. The Roughness of the coating Ra<0.01